OVERVIEW: The 304 stainless steel ammonia absorber and circulation tank experience temperatures of up to 100°C and an aggressive Chemical environment.
The prevention of stress corrosion pitting was achieved in the heat affected areas by applying corrosion protection on the entire internal surface.
INDUSTRY
ENVIRONMENT
Normal operating temperature is 60-70°C. Excursions up to 100°C are common.
• Wet ammonia gas
• Diluted sulphuric acid (up to about 20%)
• Ammonium sulphate
• Naphthalene
• Benzene
• Aromatic and aliphatic hydrocarbons
• Hydrogen sulphide
• Hydrogen cyanide
SUBSTRATE
304 Stainless Steel – Ammonia absorber and circulation tank
CHALLENGE
Prevent Stress Corrosion Pitting in the heat effected areas, these are generally found either side at the toe of the weld. Apply corrosion protection on the entire internal surfaces within a 72 hours outage
SOLUTION
Abrasive blast to Chemcote’s Specifications and 3 coats of Chem-tect™ RF 300 Series
SCOPE
Recommend the entire internal surfaces are treated
Mobilise on site
Set up of dust containment only
Set up of De-humidification equipment
Abrasive blast to Chemcote Standards
Application of a Chem-tect™ RF 300 in 3 coats including strip coat all difficult to reach areas
De-mobilise from site
PRODUCTS
Chem-tect™ RF 364 – vinyl ester / acrylic co-polymer enhanced with flaked glass; very suitable for immersed environments where superior resistance to chemical attack is required
OUTCOME
The best outcome the asset owner has obtained after years of trials using various epoxies and fibreglass linings. The combined large anchor profile achieved while abrasive blasting and excellent permeation resistance of the glass flake filler has proven itself again.
RELATED CASE STUDIES
Air Receiver Restoration for Long-Term Durability
Pitting corrosion near shaft landing After first abrasive blasting After 2nd Abrasive blast holes were found requiring composite reinforcement Filling void in difficult to reach
High Performing Replacement for 316L SS
On inspection flange corrosion Deep pitting on forged section Application of 1st coat Ready to be put into service for 25+ years of life OVERVIEW:
Power Station Debris Filter Lining Repair
Damage to existing rubber lining Internal void to be filled in around the circumference of the screen Close up of repair area for the full